KINKOU-Uea keleawe Beryllium Kiekie (C17200)
1. Ka Hoʻohui Kimia o KINKOU-Kūpono KiʻekiʻeUea keleawe Beryllium
Hoʻohālike | Be | Ni+Co | Ni+Co+Fe | Ni+Co+Fe+Be+Cu |
C17200 | 1.8-2.0 | ≥0.20 | ≤0.6 | ≥99.5 |
2. Na Pono Kino o KINKOU-Pono KiekieUea keleawe Beryllium
Anawaena | Ikaika U'i (MPa) |
≤φ0.20mm | 784-1078 |
>φ0.20mm | 686-980 |
3. Ana a Allowable Deviation o KINKOU-High PrecisionBeryllium CopperUea
Nui | φ0.03-φ0.09 | φ0.10-φ0.29 | φ0.30-φ1.0 |
ʻAe ʻia ʻo Deviation | -0.003 | -0.005 | -0.01 |
ʻōpuni | ʻAʻole e ʻoi aku ke anawaena ma mua o ka palena ʻae ʻia |
4. Noi o KINKOU-High PrecisionBeryllium CopperUea
Hoʻohana nui ʻia ia no ka puna uea, twist-pin, pihi fuzz, manamana lima, a me nā huahana hoʻohui kiʻekiʻe.
E kākau i kāu leka ma aneʻi a hoʻouna mai iā mākou